Chemical Composition
0.75 to 0.85
%    
11 to 13
%    
4 to 4.75
%    
56.4 to 63.5
%    (estimate)
0.2 to 0.4
%    
0.4 to 1
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.2 to 0.4
%    
1.5 to 2.1
%    
18.5 to 21
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
302
 (maximum)  
 
Other Information