Range attributes
0.38 to 0.45
%    
0.9 to 1.2
%    
96.8 to 97.9
%    (estimate)
0.5 to 0.8
%    
0.15 to 0.3
%    
0.025
%    
0.025
%    
0.15 to 0.4
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Austria
ONORM M3170
 
Long text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 