Chemical Composition
0.25
%  (maximum)  
0.15
%  (maximum)  
0.35
%  (maximum)  
97.5 to 100
%    (estimate)
1.35
%  (maximum)  
0.06
%  (maximum)  
0.008
%  (maximum)  
0.2
%  (maximum)  
0.035
%  (maximum)  
0.04
%  (maximum)  
0.008
%  (maximum)  
0.008
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
275
MPa  (minimum)  
380
MPa  (minimum)  
15 to 20
% strain    
 