Chemical Composition
0.47 to 0.55
%    
0.8 to 1.1
%    
96.7 to 97.8
%    (estimate)
0.65 to 0.95
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.15 to 0.35
%    
0.15 to 0.25
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1080
MPa  (minimum)  
1230
MPa  (minimum)  
10
% strain  (minimum)  
363 to 429
   
 
Other Information