Chemical Composition
2.6
%  (maximum)  
1 to 1.5
%    
0.5
%  (maximum)  
58.3 to 69
%    (estimate)
0.5 to 1.5
%    
28 to 32
%    
0.08
%  (maximum)  
0.5
%  (maximum)  
1.5 to 3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
210
MPa    
370 to 440
MPa    
13
% strain    
130 to 190
   
 