Chemical Composition
3
%  (maximum)  
0.5
%  (maximum)  
0.5
%  (maximum)  
65.9 to 76.5
%    (estimate)
1.5 to 2.5
%    
21 to 24
%    
0.08
%  (maximum)  
0.5
%  (maximum)  
1 to 3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
170
MPa    
370 to 440
MPa    
20
% strain    
130 to 170
   
 
Other Information