Chemical Composition
0.01
%  (maximum)  
28 to 30
%    
0.15
%  (maximum)  
62.6 to 66.5
%    (estimate)
0.3
%  (maximum)  
3.5 to 4.2
%    
0.02
%  (maximum)  
2 to 2.5
%    
0.025
%  (maximum)  
0.02
%  (maximum)  
0.2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
55.1 to 60.2
ksi    
70.3 to 75.4
ksi    
15 to 20
% strain    
 