Chemical Composition
0.025
%  (maximum)  
24.5 to 26
%    
63.1 to 68.5
%    (estimate)
1
%  (maximum)  
3.5 to 4.5
%    
0.035
%  (maximum)  
3.5 to 4.5
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
0.75
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
515
MPa  (minimum)  
620
MPa  (minimum)  
20
% strain  (minimum)  
269
 (maximum)  
 
Other Information