Chemical Composition
0.05
%  (maximum)  
24 to 26
%    
0.5 to 1
%    
57.6 to 65.8
%    (estimate)
1
%  (maximum)  
3 to 4
%    
0.2 to 0.3
%    
6 to 8
%    
0.03
%  (maximum)  
0.01
%  (maximum)  
1
%  (maximum)  
0.5 to 1
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
550
MPa  (minimum)  
750
MPa  (minimum)  
25
% strain  (minimum)  
300
 (maximum)  
 
Other Information
Links



No warranty is given for the accuracy of these data