Chemical Composition
0.03
%  (maximum)  
24 to 26
%    
0.5
%  (maximum)  
58.1 to 66.8
%    (estimate)
1.2
%  (maximum)  
3 to 5
%    
0.24 to 0.32
%    
6 to 8
%    
0.035
%  (maximum)  
0.02
%  (maximum)  
0.8
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
550
MPa  (minimum)  
800
MPa  (minimum)  
15
% strain  (minimum)  
310
 (maximum)  
 
Other Information
Links