Chemical Composition
0.15
%  (maximum)  
16 to 18
%    
67.5 to 75
%    (estimate)
5.5 to 7.5
%    
0.25
%  (maximum)  
3.5 to 5.5
%    
0.06
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
275
MPa  (minimum)  
515
MPa  (minimum)  
40
% strain  (minimum)  
 
Other Information
Links