Chemical Composition
0.07
%  (maximum)  
15 to 17.5
%    
3 to 5
%    
70.4 to 79
%    (estimate)
1
%  (maximum)  
3 to 5
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
520 to 1170
MPa    
795 to 1310
MPa    
10 to 18
% strain    
255 to 388
   
 
Other Information