Chemical Composition
0.82 to 0.92
%    
0.5
%  (maximum)  
3.8 to 4.5
%    
78.8 to 82.9
%    (estimate)
0.4
%  (maximum)  
4.8 to 5.3
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.4
%  (maximum)  
1.7 to 2.1
%    
6 to 7
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 