Chemical Composition
0.73 to 0.83
%    
0.5
%  (maximum)  
3.8 to 4.5
%    
72.9 to 77.6
%    (estimate)
0.4
%  (maximum)  
0.7
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.4
%  (maximum)  
0.9 to 1.2
%    
17 to 18.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 