Chemical Composition
0.015
%  (minimum)  
0.18
%  (maximum)  
97.4 to 100
%    (estimate)
1.6
%  (maximum)  
0.09
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.5
%  (maximum)  
0.22
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
380
MPa    
500 to 640
MPa    
25
% strain    
 