Chemical Composition
0.1
%  (maximum)  
0.3
%  (maximum)  
0.3
%  (maximum)  
96.8 to 98.8
%    (estimate)
1.2 to 1.6
%    
0.04
%  (maximum)  
0.3
%  (maximum)  
0.02
%  (maximum)  
0.02
%  (maximum)  
0.5
%  (maximum)  
0
%  (maximum)  
0
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
370
MPa  (minimum)  
530
MPa  (minimum)  
21
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®