Chemical Composition
3 to 3.6
%    
1.4 to 2.4
%    
86.4 to 91.8
%    (estimate)
0.3 to 0.7
%    
0.5
%  (maximum)  
3.3 to 5
%    
0.3
%  (maximum)  
0.3
%  (maximum)  
0.2 to 0.8
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
280 to 350
MPa    
45 to 62
   
 
Other Information