Chemical Composition
2.3 to 3.6
%    
14 to 17
%    
73.4 to 80.4
%    (estimate)
0.5 to 1.2
%    
1.8 to 2.2
%    
0.8 to 1.2
%    
0.3
%  (maximum)  
0.3
%  (maximum)  
0.2 to 0.8
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
450 to 1000
MPa    
39 to 62
   
 
Other Information
Links



No warranty is given for the accuracy of these data