Chemical Composition
3 to 3.8
%    
1 to 2
%    
89.8 to 94
%    (estimate)
1
%  (maximum)  
0.3
%  (maximum)  
0.12
%  (maximum)  
2 to 3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 