Chemical Composition
0.26 to 0.34
%    
1.8 to 2.2
%    
93.7 to 95.5
%    (estimate)
0.3 to 0.6
%    
0.3 to 0.5
%    
1.8 to 2.2
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
700
MPa    
900 to 1100
MPa    
12
% strain    
 
Other Information