Chemical Composition
0.32 to 0.39
%    
1.3 to 1.7
%    
94.6 to 96.4
%    (estimate)
0.5 to 0.8
%    
0.15 to 0.3
%    
1.3 to 1.7
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
600
MPa    
800 to 950
MPa    
13
% strain    
 