Chemical Composition
2 to 2.75
%    
9 to 11
%    
27 to 31
%    
8
%  (maximum)  
0.5
%  (maximum)  
29.7 to 47.5
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.5 to 1
%    
14 to 16
%    
Ni is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links



No warranty is given for the accuracy of these data