Chemical Composition
0.15
%  (maximum)  
11.5 to 13.5
%    
83.8 to 88.5
%    (estimate)
1
%  (maximum)  
0.5
%  (maximum)  
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207
MPa  (minimum)  
414
MPa  (minimum)  
20
% strain  (minimum)  
207
 (maximum)  
 
Other Information