Chemical Composition
0.08
%  (maximum)  
17 to 20
%    
63.3 to 74
%    (estimate)
2
%  (maximum)  
9 to 13
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
207
MPa  (minimum)  
517
MPa  (minimum)  
35
% strain  (minimum)  
192
 (maximum)  
 