Chemical Composition
0.25 to 0.32
%    
97.6 to 98.4
%    (estimate)
1.3 to 1.65
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
600
MPa    
800 to 950
MPa    
13
% strain    
 