Chemical Composition
0.17 to 0.25
%    
11 to 13
%    
83.3 to 86.6
%    (estimate)
0.5 to 0.8
%    
0.8 to 1
%    
0.5 to 0.8
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.17 to 0.37
%    
0.3 to 0.45
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
590
MPa    
800 to 950
MPa    
12
% strain    
 
Other Information