Chemical Composition
2.2 to 2.9
%    
93.6 to 96.7
%    (estimate)
0.15 to 1.25
%    
0.02 to 0.15
%    
0.02 to 0.2
%    
0.9 to 1.9
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
310
MPa  (minimum)  
448
MPa  (minimum)  
4
% strain  (minimum)  
163 to 217
   
 
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®