Chemical Composition
3
%  (maximum)  
2.5 to 3.5
%    
5.5 to 7.5
%    
63.2 to 77
%    (estimate)
0.5 to 1.5
%    
13.5 to 17.5
%    
0.5
%  (maximum)  
0.5
%  (maximum)  
1 to 2.8
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
190 to 240
MPa    
1
% strain    
150 to 250
   
 
Other Information