Chemical Composition
0.15
%  (maximum)  
0.5 to 1
%    
0.2 to 0.5
%    
95.6 to 98.9
%    (estimate)
1.3
%  (maximum)  
0.3
%  (maximum)  
0.3 to 0.6
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
355
MPa    
490 to 630
MPa    
21 to 23
% strain    
 
Other Information
Links