Chemical Composition
0.015 to 0.06
%    
0.17
%  (maximum)  
0.3
%  (maximum)  
0.25
%  (maximum)  
97 to 100
%    (estimate)
1.2
%  (maximum)  
0.1
%  (maximum)  
0.0012
%  (maximum)  
0.05
%  (maximum)  
0.3
%  (maximum)  
0.025
%  (maximum)  
0.02
%  (maximum)  
0.4
%  (maximum)  
0.04
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
42.1 to 63.8
ksi    
60.2
ksi  (minimum)  
21
% strain  (minimum)  
 