Chemical Composition
0.015 to 0.06
%    
0.2
%  (maximum)  
98.1 to 100
%    (estimate)
1.15
%  (maximum)  
0.03
%  (maximum)  
0.03
%  (maximum)  
0.4
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
245
MPa  (minimum)  
415 to 555
MPa    
22
% strain  (minimum)  
 
Other Information