Chemical Composition
0.1 to 0.17
%    
16 to 18
%    
77.3 to 82.4
%    (estimate)
1
%  (maximum)  
1.5 to 2.5
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
680
MPa    
880 to 1080
MPa    
11
% strain    
 
Other Information