Chemical Composition
0.02 to 0.06
%    
0.1 to 0.18
%    
0.7 to 1
%    
0.35
%  (maximum)  
95.9 to 98.1
%    (estimate)
0.4 to 0.9
%    
0.45 to 0.55
%    
0.01 to 0.06
%    
0.35
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
0.15 to 0.4
%    
0.02 to 0.06
%    
0.02 to 0.1
%    
0.015 to 0.06
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
270
MPa    
440 to 580
MPa    
20
% strain    
 