Chemical Composition
0.02 to 0.06
%    
0.14 to 0.2
%    
0.35
%  (maximum)  
95.7 to 99.6
%    (estimate)
1.5
%  (maximum)  
0.01 to 0.06
%    
1.2
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
0.2 to 0.6
%    
0.02 to 0.06
%    
0.02 to 0.1
%    
0.015 to 0.06
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
355
MPa    
510 to 650
MPa    
19
% strain    
 