Chemical Composition
0.02 to 0.06
%    
0.22
%  (maximum)  
0.35
%  (maximum)  
97 to 99.3
%    (estimate)
0.5 to 1.3
%    
0.01 to 0.06
%    
0.35
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
0.15 to 0.4
%    
0.02 to 0.06
%    
0.02 to 0.1
%    
0.015 to 0.06
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
255
MPa    
440 to 550
MPa    
20
% strain    
 
Other Information
Links



No warranty is given for the accuracy of these data