Chemical Composition
0.35 to 0.45
%    
0.9 to 1.2
%    
96.8 to 98
%    (estimate)
0.5 to 0.8
%    
0.2 to 0.35
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.1 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
750
MPa  (minimum)  
990 to 1140
MPa    
10
% strain  (minimum)  
285 to 341
   
 
Other Information