Chemical Composition
1 to 1.1
%    
3.75 to 4.5
%    
77.5 to 82.9
%    (estimate)
0.15 to 0.4
%    
4.75 to 6.5
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.2 to 0.45
%    
2.25 to 2.75
%    
5 to 6.75
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
223 to 255
   
 