Chemical Composition
0.22
%  (maximum)  
0.2
%  (minimum)  
98.2 to 98.9
%    (estimate)
0.85 to 1.25
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.3
%  (maximum)  
0.02
%  (minimum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
345
MPa  (minimum)  
485
MPa  (minimum)  
22
% strain  (minimum)  
 
Other Information