Chemical Composition
0.85 to 0.92
%    
7.75 to 8.75
%    
3.5 to 4.2
%    
71.8 to 76.6
%    (estimate)
0.4
%  (maximum)  
8 to 9.2
%    
0.03
%  (maximum)  
0.03
%  (maximum)  
0.45
%  (maximum)  
1.8 to 2.2
%    
1.5 to 2
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 