Range attributes
0.25 to 0.5
%    
23 to 26
%    
8
% strain  (minimum)  
55.2 to 64.8
%    (estimate)
2.5
%  (maximum)  
12 to 14
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1.75
%  (maximum)  
490
MPa  (minimum)  
235
MPa  (minimum)  
 
Discrete attributes
Short text attributes
HRSC 13A-CF
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
South Korea
Centrifugal cast steel pipe; add CF suffix.
HRSC 13A
KS D 4105
 
Long text attributes
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Centrifugal cast steel pipe; add CF suffix.
 