Chemical Composition
0.2 to 0.5
%    
26 to 30
%    
53.9 to 65.8
%    (estimate)
2
%  (maximum)  
0.5
%  (maximum)  
8 to 11
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
275
MPa  (minimum)  
585
MPa  (minimum)  
9
% strain  (minimum)  
 