Chemical Composition
0.7 to 1.2
%    
0.12
%  (maximum)  
17 to 20
%    
75.5 to 81.5
%    (estimate)
1
%  (maximum)  
0.6
%  (maximum)  
0.04
%  (maximum)  
0.03
%  (maximum)  
0.8 to 1.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
270
MPa    
15
% strain    
212
 (maximum)  
 
Other Information
Links



No warranty is given for the accuracy of these data