Chemical Composition
0.08
%  (maximum)  
25 to 28
%    
46.3 to 54
%    (estimate)
1 to 2.5
%    
20 to 22.5
%    
0.03
%  (maximum)  
0.02
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information