Chemical Composition
0.08
%  (maximum)  
18 to 21
%    
57.3 to 71
%    (estimate)
1.5
%  (maximum)  
2 to 3
%    
1
%  (maximum)  
9 to 13
%    
0.04
%  (maximum)  
0.035
%  (maximum)  
2
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information