Chemical Composition
0.07
%  (maximum)  
16 to 18
%    
59.4 to 67.5
%    (estimate)
2
%  (maximum)  
4 to 5
%    
12.5 to 14.5
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
185
MPa    
440 to 640
MPa    
20
% strain    
 