Chemical Composition
0.07
%  (maximum)  
22 to 23
%    
0.3
%  (maximum)  
62.1 to 66.5
%    (estimate)
1.5 to 2
%    
0.75
%  (maximum)  
9.5 to 10.5
%    
0.035
%  (maximum)  
0.025
%  (maximum)  
0.5 to 1.2
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 