Chemical Composition
0.03
%  (maximum)  
19 to 21
%    
1.5 to 2
%    
45.2 to 52.9
%    (estimate)
1
%  (maximum)  
2.5 to 3.5
%    
0.1 to 0.2
%    
24 to 26
%    
0.035
%  (maximum)  
0.02
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
200
MPa    
440 to 640
MPa    
20
% strain    
 