Chemical Composition
0.9 to 1.3
%    
27 to 30
%    
65.6 to 72.1
%    (estimate)
1
%  (maximum)  
0.045
%  (maximum)  
0.03
%  (maximum)  
2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
880 to 1080
MPa    
260 to 330
   
 
Other Information