Chemical Composition
0.27 to 0.34
%    
0.3
%  (maximum)  
97.4 to 98.4
%    (estimate)
1.2 to 1.5
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.15 to 0.4
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
440
MPa    
690 to 830
MPa    
15
% strain    
 