Chemical Composition
0.001 to 0.005
%    
0.12 to 0.21
%    
0.85 to 1.2
%    
95.4 to 96.7
%    (estimate)
0.45 to 0.7
%    
0.45 to 0.6
%    
1.2 to 1.5
%    
0.035
%  (maximum)  
0.035
%  (maximum)  
0.2 to 0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
620
MPa  (minimum)  
725 to 930
MPa    
14
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data